A 82一 Fig 4 Hot-rolled 1022 steel showing severe banding. Bands of pearlite(dark) and ferrite were caused by segregation of carbon and other elements during solidification and later decomposition of austenite. Nital. 250x. Courtesy of J.R. Kilpatrick Thefileisdownloadedfromwww.bzfxw.comFig. 4 Hot-rolled 1022 steel showing severe banding. Bands of pearlite (dark) and ferrite were caused by segregation of carbon and other elements during solidification and later decomposition of austenite. Nital. 250×. Courtesy of J.R. Kilpatrick The file is downloaded from www.bzfxw.com