表3用氢还原APT时的物相和颜色的变化与还原温度的关系 Table 3 The variation of the phases and colour of the samples reduced from APT by hydrogen at various temperature Reduction Samples temperature Colour phases 心 A-0 275 baby bine-black nonecystalline ATB A-1 325 blue-black tetragonal ATB, hexagonal ATB A-2 hexagonal ATB. 375 pale blue tetragonal ATB A-3 425 blue hexagonal ATB, tetragonal ATB,W2 00ss A-4 450 加Azarine 7多c058, hexagonal ATB, tetragonal ATB A-5 475 blue-purpe Wa00ss,hexagonal ATB, tetragonal ATB A-6 500 purple-blue abid A-7 525 abid W:0058,ATB,B-W,WOa A-8 575 pale brown WO2,8-W,a-W,W:005a (trace) A-9 625 dark brown W02,a-W,B- A-10 675 grey-brown a-W,WO2,B-W A-11 725 dark grey a-W,WO: 表4用氢还原WO,时的物相和颤色的变化与还原温度的关系 Table 4 The variation of the phases and colour of the samples reduced from WO,by hydrogen at various temperature Reduction Remark& Samples temperature Colonr phases column t Y-1 375 blue-green WO The sample ¥-2 425 blue WOa,W200s8 Y-6,Y-7, Y-3 475 过azarine W20058,W18049 and Y-8 W0。,W02(trace) have been Y-4 525 purple-blue W:0058,1s04g,W0g analysed Y-5 575 brown W02 quantitatily ¥-6 625 brown W02(92.5%),a-W(65), B-W(1.5%) Y-7 655 dark brown W02(76.89%),x-W(23.1%) B-W(trace) Y-8 705 grey-brown a-w(72.97%),W0z(27.03%) 痕量。高于625℃α-W量随温度升高迅速增加。这与A组相-一致的结果说明,当还原温 40表 用 氮还原 时 的物相和颜色的变化与 还 原温度 的关系 亡 沁。 ,” 气 , ℃ 一一 一一 一一 一 一 一 一一 一 一 一 一 一 一一 一 人, 七 么 一 人一 果娜 人· · 一 一 一 盗宾二默 欣 义 , 。 ‘ 恤 一 -,一下石斌不下雨面丽门丽币一 理 吐 · 黑 至 一 一 , 。 , ,月 , 一 一 一一 一 一一 一 一 一 一一 , 一 一 。 卜 七 一 , 月 一 , 一 , 。 ,“ 一 , 月一 “ 一 , , 月 一 人· “ 一 一 表 用 氮还原 时 的物相和颇 色的变化与 还原温度的关系 。 , ℃ , 拍 一 五 一 一 ‘ 。 、 。 ‘ , 。 。 一 “ ‘ 二“ · 欲拓麒 黔 一 一 , ‘ , , 一 卜 一 “ “ ,, 黔思黔 ,“ 一 一 灿 ‘ 价 黔 蹂黔 ’ , 一 ‘ · ‘ 殉 一 了 ‘ 卜 , 一 拓 , 多 痕量 。 高于 ℃ 一 量 随温度 升高迅速增加 。 , 这 与 组 相一 致的结果说 明 , 当还 原 温
<<向上翻页向下翻页>>
©2008-现在 cucdc.com 高等教育资讯网 版权所有